FWIW, I have completed alodyning (using a shaped "bath" lined with plastic)
and am planning on painting with zinc oxide followed by enamel spray.
Anodizing is another possibility but I had the same concerns as you about
stones -- you can't touch it up like paint.
Best regards,
Nick Hammond
-----Original Message-----
Subject: landing gear
What have folk done with their swinging arm (LG02) in terms of corosion
protection etc. I've used alodine on all the small parts but given that this
is hanging down in all the c**p and likely to be subject to stones etc I was
wondering about something more durable - possibly powder coating. Any
thoughts
Regards Paul Stewart #432
|