Brad,
Sand the gel coat slightly befor applying Smooth Prime - it will stick
better. After applying Smooth Prime everywhere, you will see that the gel
coat surface is far from perfect. "Moutains" and "valleys" show up, if you
cover the first coats of Smooth Prime with a black powder (3M has a perfect
product) and then sand the surface.
Regards,
Alfred
_____
Von: owner-europa-list-server@matronics.com
[mailto:owner-europa-list-server@matronics.com] Im Auftrag von Brad Shafer
Gesendet: Samstag, 11. November 2006 22:49
An: europa-list@matronics.com
Betreff: Europa-List: UV Smooth Prime
Simple question. Should UV Smooth Prime be used on all surfaces including
the surfaces that have a white coating (gel coat?) from the factory? Or
just the "raw" fiberglass (blue) surfaces?