I have a good bond everywhere except an are about 1.5 inches long but about
1/2 inch which is to say that I have 1.5 inches with just 1/4 inch of
bond. This is on the forward edge of the door plexi.
I tried drilling and injecting from the back but it appears it's not a void
but a de-lamination and the glue wont flow in.
So what I was thinking it to do a 2 ply lay up over the joint between the
door and the forward edge of the plexi ith araldite forming the the bond
between the bid and the plexi. Does anyone have a comment on this?
Thanks
Will
HJ 460
PS started the engine/airmaster over the weekend with the Dynon connected
everything works! And my 14 year project has a name "HJ 460" and I have a
trailer.
William Daniell
LONGPORT
+57 310 295 0744
|