Prev (6 of 12)
 
Next (8 of 12)
7 of 12: *
The sharp curve at the leading edge caused the laminations to lift, leaving two voids below the surface. A few holes were drilled, and flox was injected into the large void; pure epoxy was injected into the smaller one.
Prev (6 of 12)
 
Next (8 of 12)