>> I heard about some people having problems with Poly Fiber just as I was about to apply Top Gloss. The UK distributor advised that the problem was due to moisture content in the (UV) Smooth Prime. This is a different problem to the disbond problem. If the moisture in smooth prime is not allowed to vapourise out completely then any coating you put on top can blister. The best thing to do is leave the Smooth Prime for a month or so in warm weather to allow it to dry properly before applying the top coating. Tony |