We use Rustoleum Hammerite spray on many things in the shop. It looks OK a
nd it is easy to touch up. It is great for fiberglass components as it cov
ers small imperfections well. It doesn't hold up to heat well=2C but has b
een used on the ducting in the cowl.
We have not used it on metal control brackets or rods as I like a smooth fi
nish to identify corrosion bubbles hidden under the paint.
It has earned our "dammed adequate" recommendation.
Bud
Sent from my Verizon Wireless 4G LTE DROID
On Feb 25=2C 2015 12:59 PM=2C tennant <barrington.tennant@gmail.com> wrote:
Rowland=2C
2 coats of Hammerite - 17 years ago and the TW spring still looks OK!
Whatever you use must be quite flexible to resist those one in 20 "not so p
erfect" landings!!
Barry
--------
Barry Tennant
D-EHBT
At EDLM - Germany
Read this topic online here: